Material Notes:
This is an extremely low 325 Mesh wet residue clay. It can be employed in a variety of applications where high purity mineral filler is required. It has a moderate GE brightness value and is particularly beneficial where suspension of other materials is important or where low settling tendency is critical.Information provided by Old Hickory Clay Company
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Brightness 69 %
69 %
GE Brightness
Oil Absorption 40 %
40 %
Moisture Absorption <= 2.00 %
<= 2.00 %
Particle Size 0.40 µm
0.40 µm
Median particle diameter
0.50 µm
0.50 µm
57% of particles less than
1.0 µm
1.0 µm
68% of particles less than
2.0 µm
2.0 µm
77% of particles less than
5.0 µm
5.0 µm
90% of particles less than
10 µm
10 µm
96% of particles less than
<= 20 µm
<= 20 µm
99% of particles less than
pH 6.0
6.0
Component Elements Properties Metric English Comments
Al2O3 29.2 %
29.2 %
CaO 0.090 %
0.090 %
Fe2O3 0.81 %
0.81 %
K2O 0.12 %
0.12 %
Loss on Ignition(%) 9.8 %
9.8 %
MgO 0.19 %
0.19 %
Na2O 0.54 %
0.54 %
SiO2 56.4 %
56.4 %
TiO2 2.26 %
2.26 %
Descriptive Properties Value Comments
Crude Color Cream, White, Tan
Wet Sieve Residue (%) 0.5
Wet Sieve Residue, +325 mesh