Oceanchem Group Calcium Chloride 74-77% flakes

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group Calcium Chloride 74-77% flakes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molecular Formula: CaCl2Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Particle Size 5000 - 20000 µm
5000 - 20000 µm
Descriptive Properties Value Comments
Calcium Hydroxide (%) <0.15
Insoluble (%) <0.1
Water insoluble
Molecular Formula CaCl2
Purity (%) 74-77
Sodium and Alkaline salts (%) <4
Sulphate (%) <0.05