Oceanchem Group BRONOPOL

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group BRONOPOL.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molecular Formula: C3H6BrNO4Cas No.: 52-51-7Usage: Bactericide, it is widely used in industrial circulating water, algae-killing, paper pulp, paint, plastic, timber-cooling circulating water and other industries. In addition, it can be used to prevent daily-used cosmetic products from moldly and corrosion.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Molecular Weight 200 g/mol
200 g/mol
Thermal Properties Metric English Comments
Melting Point 126 - 131 °C
259 - 268 °F
Descriptive Properties Value Comments
Assay (%) >99
CAS Number 52-51-7
Index No. GSAL-WT-BRONOPOL
Loss on Drying (%) <0.5
Molecular Formula C3H6BrNO4