Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oceanchem Group ANTIOXIDANT SK-900

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group ANTIOXIDANT SK-900.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cas No.: 2082-79-3Properties: Antioxidant SK-900 is a kind of compound components, including antioxidant SK-168 and antioxidant SK-1076. Soluble in benzene, hexane, ethyl acetate, insoluble in water.Uses: Antioxidant SK-900, with good synergistic of antioxidant SK-168 and SK-1076, can retard heated degradation and oxidative degradation of polymeric substances during processing and in end applications. It can be widely used for PE, PP, nylon, PC, ABS resin and other petro-products. The amount to be used may be 0.1-0.8%.Package and Storage: Packed with plastic bag in composite plastic woven sack, Net 25kg/bag. Sote in a cool area designed for the storage of chemicals. Period of Validity: Normally 6 months.Information Provided by Oceanchem Group
Optical Properties Metric English Comments
Transmission, Visible >= 96 %

@Wavelength 425 nm
>= 96 %

@Wavelength 425 nm
>= 97 %

@Wavelength 500 nm
>= 97 %

@Wavelength 500 nm
Descriptive Properties Value Comments
Appearance Clear white powder
CAS Number 2082-79-3
Content of Antioxidant 17.5-22.5
Antioxidant SK-1076
77.5-82.5
Antioxidant SK-168
Users viewing this material also viewed the following: