Molecular Formula: C12H18Br6Cas No.: 3194-55-6Characteristics: The product is white crystalline powder, melting point greater than 180°C, bromine content greater than or equal to 73%. This product is soluble in alcohols, ketones andesters, such as organic solvents such as methanol, ethanol, amyl acetate, acetone and so on. This product should be stored in a cool, dry, ventilated warehouse, in the store and transportation process should be handled with care to prevent impact damage.Use: It is used as flammable inhibitor for EPS, polypropylene fibre and styrene resin, it is also used as an adding agent of flammable inhibitor for polyethylene, poly carbonate, unsaturated polester. It can be used in fire-proof treatment of fabric, butadiene styrene rubber, binder, coating and unsaturated polyester.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Volatiles 0.50 %

@Temperature 110 °C,
Time 7200 sec
0.50 %

@Temperature 230 °F,
Time 2.00 hour
Molecular Weight 641.7 g/mol
641.7 g/mol
Thermal Properties Metric English Comments
Melting Point 178 - 185 °C
352 - 365 °F
Ordinary type
185 - 195 °C
365 - 383 °F
High melting point
Descriptive Properties Value Comments
Bromine, Br (%) 74-75
CAS Number 3194-55-6
Hue APHA <30
Molecular Formula C12H18Br6