Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® Vexel™ B12GF45 , 45% Glass Reinforced PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
Manufacturer Nylene®
Trade Name Vexel™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® Vexel™ B12GF45 , 45% Glass Reinforced PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Vexel™ B12GF45 is a 45% glass fiber reinforced, general purpose PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.67 g/cc
1.67 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 152 MPa
22000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 227 °C
440 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648