Nylene® PA6/6 Mineral Filled 6140 HS Nylon 6/6

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Mineral Filled
Manufacturer Nylene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® PA6/6 Mineral Filled 6140 HS Nylon 6/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% Mineral Filler; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 97.0 MPa
14100 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Flexural Modulus 6.60 GPa
957 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 199 °C
390 °F
ASTM D648