Material Notes:
15% Glass Reinforced/25% Mineral Filled.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 130 MPa
18900 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Modulus 6.86 GPa
995 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 254 °C
489 °F
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
ASTM D648