Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® Naxel™ PC35CV Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Nylene®
Trade Name Naxel™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® Naxel™ PC35CV Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Naxel™ PC35CV is a 12 melt, virgin, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Melt Flow 12 g/10 min
12 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 61.4 MPa
8900 psi
ASTM D638
Elongation at Break 120 %
120 %
ASTM D638
Flexural Modulus 2.31 GPa
335 ksi
ASTM D790
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
265 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved