Nylene® 7250 C HS , 50% Glass Fiber/Ceramic Reinforced, Low Warp, High Stiffness Specialty Nylon

Category Polymer , Thermoplastic , Nylon
Manufacturer Nylene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® 7250 C HS , 50% Glass Fiber/Ceramic Reinforced, Low Warp, High Stiffness Specialty Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nylene® 7250 C HS is a 50% glass fiber/ceramic reinforced, low warp, high stiffness specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.59 g/cc
1.59 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 124 MPa
18000 psi
ASTM D638
Flexural Modulus 10.3 GPa
1500 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
420 °F
ASTM D3418