Material Notes:
Dry as molded. Extrusion grade. Nylene 607 is a very high viscosity extrusion resin having an ASTM relative viscosity of 800. Nylene 607 has excellent structural strength, durability, and physical properties. It has good melt strength and good draw-down properties which promote dimensional control for extrusion of pipe, tubing, film, and sheet. It is particularly recommended for the extrusion of thick slab, large rod stock, and large complex profiles. Optimum processing conditions should permit for a melt temperature of 550 - 575ºF at the die.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 0.020 %
0.020 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 85.0 MPa
12300 psi
ASTM D638
Elongation at Break 210 %
210 %
ASTM D638
Flexural Yield Strength 107 MPa
15500 psi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 186 °C
367 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 295 °C
563 °F