Nylene® 603 Nylon 6, Extrusion Grade

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer Nylene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® 603 Nylon 6, Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dry as molded. Extrusion grade. Nylene 603 is a plasticized, high residual monomer resin designed for extrusion applications requiring excellent flexibility, high strength and good abrasion resistance. Applications include flexible tubing, cable jacketing, and monofilament extrusion such as fish line and netting, sewing thread, and weaving thread. Optimum processing conditions should permit for a melt temperature of approximately 450ºF at the die.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 3.2 %
3.2 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 88.0 MPa
12800 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Flexural Yield Strength 61.0 MPa
8850 psi
ASTM D790
Izod Impact, Notched 1.90 J/cm
3.56 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
334 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 232 °C
450 °F