Material Notes:
Description: Nylene® 204 (HS) is a fast cycle, medium viscosity, nucleated nylon 6. 204 is UL approved and automotive approved. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 79.3 MPa
11500 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
420 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.6 °C
150 °F
ASTM D648
Users viewing this material also viewed the following: