Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, MoS2 Filled
Manufacturer Nylacast
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The combined Nylube lubrication system incorporating fine particles of molybdenum disulphide provides enhanced load bearing capabilities while retaining Nylube's excellent frictional characteristics.Information provided by Nylacast Ltd.
Physical Properties Metric English Comments
Density 1.145 g/cc
0.04137 lb/in³
method A; ISO 1183:1987
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ISO 868:2003
Tensile Strength, Yield 85.0 MPa
12300 psi
Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 20 %
>= 20 %
Type 1B, 50mm/min; ISO 527-1/2:1993
Tensile Modulus 4.20 GPa
609 ksi
Type 1B, 50mm/min; ISO 527-1/2:1993
Flexural Strength 110 MPa
16000 psi
1.5mm/min; ISO 178:2001
Flexural Modulus 3.50 GPa
508 ksi
1.5mm/min; ISO 178:2001
Compressive Strength 100 MPa
14500 psi
Type B, 5mm/min; ISO 604:2002
Compressive Modulus 2.80 GPa
406 ksi
Type B, 5mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
Type A; ISO 180:2000
Coefficient of Friction, Dynamic 0.12

@Pressure 1.75 MPa
0.12

@Pressure 254 psi
31.4m/min
K (wear) Factor 91.0 x 10-8 mm³/N-M

@Pressure 1.75 MPa
45.2 x 10-10 in³-min/ft-lb-hr

@Pressure 254 psi
31.4m/min
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2:1999
Maximum Service Temperature, Air 185 °C
365 °F
Intermittent
115 °C

@Time 1.80e+7 sec
239 °F

@Time 5000 hour
Continuous
Minimum Service Temperature, Air -100 °C
-148 °F
Intermittent
-40.0 °C
-40.0 °F
Continuous
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+15 ohm-cm
5.00e+15 ohm-cm
IEC 60093:1980-01
Surface Resistance 5.00e+12 ohm
5.00e+12 ohm
IEC 60093:1980-01
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
IEC 60250:1969-01
4.0

@Frequency 100 Hz
4.0

@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 29.0 kV/mm
737 kV/in
IEC 60243-1:1998-01
Comparative Tracking Index 604 V
604 V
IEC 60112:2003-01
Descriptive Properties Value Comments
Color Black
Wear Rate 0.08 mg/km
31.4m/min, 1.75MPa