Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nye Lubricants 369VF Grease

Category Fluid , Lubricant , Lithium Gellant , Organic Soap Gellant , Polyalphaolefin (PAO)
Manufacturer Nye Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 369VF Grease.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 145
145
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 390 cSt
390 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 39 cSt
39 cSt
Base Oil; ASTM D445
Evaporation Loss <= 1.0 %
<= 1.0 %
ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 230
230
ASTM D217
Penetration P(60), 1/10 mm 265
265
ASTM D217
Oil Separation <= 5.0 %
<= 5.0 %
FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Recommended
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Recommended
Pour Point -30.0 °C
-22.0 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PAO
Gellant Type Li soap
Users viewing this material also viewed the following: