Nye Lubricants 131A (DMO) Delicate Machinery Oil

Category Fluid , Lubricant , White Mineral Oil (WMO)
Manufacturer Nye Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 131A (DMO) Delicate Machinery Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 125
125
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 15 cSt
15 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 3.6 cSt
3.6 cSt
Base Oil; ASTM D445
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Recommended
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Recommended
Pour Point -30.0 °C
-22.0 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type WMO