NuSil R-2185 Silicone Two Part Sealing & Adhesive

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer NuSil
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NuSil R-2185 Silicone Two Part Sealing & Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Purpose: Two Part Sealing & AdhesiveComments: Flowable, Light-weight ElastomerCure System: PlatinumInformation provided by NuSil
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
Viscosity 96000 cP
96000 cP
A
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Tensile Strength at Break 3.40 MPa
493 psi
Elongation at Break 580 %
580 %
Tear Strength 11.4 kN/m
65.0 pli
Processing Properties Metric English Comments
Cure Time 60.0 min
1.00 hour
Work Time
30.0 min

@Temperature 150 °C
0.500 hour

@Temperature 302 °F
Descriptive Properties Value Comments
Color White
Mix Ratio 10:1