Material Notes:
Description: Low consistency elastomers (LCEs) are useful alternatives to liquid silicone rubber (LSR) and high consistency rubber (HCR) for end users who need a low viscosity elastomer which provides other unique properties. LCEs lend themselves to applications that require a pourable, selfleveling silicone. Applications include: encapsulating a device, backfilling a void, potting an electronic component that cannot withstand exposure to high heat, or prototyping a mold. Features of low consistency elastomers may include the following: Optically clearSelf-levelingLow and high temperature cureLow viscosityEasy to processComments: Low Viscosity, High DurometerCure System: PlatinumInformation provided by NuSil