Material Notes:
Description: Liquid silicone rubbers, or LSRs, are elastomer systems reinforced with silica. They contain functional polymers of lower average molecular weight and viscosity when compared to high consistency rubbers (HCRs). They are typically supplied as two-component systems and formulated in a 1:1 mix ratio. Because their consistency is akin to petroleum jelly, they are often pumped with injection molding equipment to form molded components such as o-rings, gaskets, valves, seals, and other precision molded parts.Important Properties of Adhesives: LSRs are designed for liquid injection molding (LIM) processes which may utilize single or multi-cavity molds, or for overmolding processes. Originally designed for automated systems, they are developed with high volume applications in mind and benefit from their high strength. Features of liquid silicone rubbers include the following: Ideal for high throughput manufacturingPlatinum cure system—no post cure requiredTypical work time in excess of 72 hoursCure rapidly at elevated temperaturesEasily pigmented using NuSil color masterbatchesComments: FluorosiliconeCure System: PlatinumInformation provided by NuSil
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Typical
35 - 50
35 - 50
Certified
Tensile Strength at Break 5.50 MPa
798 psi
Certified
7.90 MPa
1150 psi
Typical
Elongation at Break 175 %
175 %
Certified
335 %
335 %
Typical
Tear Strength 3.51 kN/m
20.0 pli
Certified
10.5 kN/m
60.0 pli
Typical
Processing Properties Metric English Comments
Extrusion Rate 3.75 g/min
3.75 g/min
Cure Time 30.0 min

@Temperature 150 °C
0.500 hour

@Temperature 302 °F
>= 1440 min

@Temperature 25.0 °C
>= 24.0 hour

@Temperature 77.0 °F
Work Time
Descriptive Properties Value Comments
Mix Ratio 1:1
Copyright © lookpolymers.com All Rights Reserved