Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NuSil MED-4065 Silicone, Two Part High Consistency Elastomer - Restricted Medical Use

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer NuSil
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NuSil MED-4065 Silicone, Two Part High Consistency Elastomer - Restricted Medical Use.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High consistency rubber, or HCR, consists of high molecular weight polymer combined with silica to produce a material that can be molded, extruded, or calendared into a useful end product. An HCR has the consistency of clay and is primarily formulated in a one or two part system (peroxide and platinum catalysts respectively).Important Properties: Most platinum cure high consistency rubbers are two component systems with an easy-to-work-with 1:1 mix ratio. Features of platinum cure high consistency rubbers include the following: Two part (typically)Heat acceleratedNo byproductsPost cure optionalLow percent shrinkageComments: High TearCure System: PlatinumInformation provided by NuSil
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Typical
60 - 70
60 - 70
Certified
Tensile Strength at Break 4.80 MPa
696 psi
Certified
7.90 MPa
1150 psi
Typical
Tensile Stress 2.41 MPa

@Strain 200 %
350 psi

@Strain 200 %
Elongation at Break 700 %
700 %
Certified
950 %
950 %
Typical
Tear Strength 6.14 kN/m
35.0 pli
Certified
7.73 kN/m
44.1 pli
Typical
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 116 °C
0.167 hour

@Temperature 241 °F
150 min

@Temperature 25.0 °C
2.50 hour

@Temperature 77.0 °F
Work Time
Descriptive Properties Value Comments
Mix Ratio 1:1
Plasticity 130 mils