NuSil MED-1356 Silicone, One Part Adhesive/Sealant - Restricted Medical Use

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer NuSil
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NuSil MED-1356 Silicone, One Part Adhesive/Sealant - Restricted Medical Use.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Silicone adhesives are elastomers or pressure sensitive adhesive systems that are designed to bond silicone surfaces to each other and to other substrate surfaces such as metals and plastics. There are one-part and two-part adhesives, ranging in consistency from flowable to non-flowable (non-slump). Silicone primers are specially formulated silanes supplied in a solvent that are used to improve the bond strength between a silicone elastomer or adhesive and another substrate surface (silicone, metals, and certain plastics). In general, silicone adhesives adhere well to substrates such as glass, aluminum, titanium, other silicones, and some ceramics. While various types of materials can be used as adhesives, silicones are consistently chosen for their many inherent properties and overall versatility. Advantages of these adhesives are as versatile as silicone itself: Proven biocompatibilityResistance to moistureAbility to remain elastic at temperatures below 0 ºCAbility to resist chemical breakdown at temperatures >200 ºCLow modulus prevents warpage, delamination and substrate failureComments: PSA/Ethyl AcetateCure System: AcetoxyInformation provided by NuSil
Physical Properties Metric English Comments
Viscosity 1370 cP
1370 cP
Descriptive Properties Value Comments
Mix Ratio 1 part