NuSil CV1-8151 Silicone Gel

Category Polymer , Thermoset , Silicone
Manufacturer NuSil
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NuSil CV1-8151 Silicone Gel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Purpose: GelsComments: Low ViscosityInformation provided by NuSil
Physical Properties Metric English Comments
Viscosity 2500 cP
2500 cP
Mechanical Properties Metric English Comments
Penetration 0.40
0.40
Processing Properties Metric English Comments
Cure Time >= 1800 min
>= 30.0 hour
Work Time
30.0 min

@Temperature 150 °C
0.500 hour

@Temperature 302 °F
Descriptive Properties Value Comments
Color Clear
Mix Ratio 1:1