NuSil CV-2963 Silicone, Thermally Conductive

Category Polymer , Thermoset , Silicone
Manufacturer NuSil
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NuSil CV-2963 Silicone, Thermally Conductive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Purpose: Two Part Adhesive and SealantCure system: PlatinumInformation provided by NuSil
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength at Break 2.90 MPa
421 psi
Elongation at Break 250 %
250 %
Shear Strength 1.90 MPa
276 psi
Lap, Primed with CF1-135
Tear Strength 8.77 kN/m
50.0 pli
Thermal Properties Metric English Comments
Thermal Conductivity 0.640 W/m-K
4.44 BTU-in/hr-ft²-°F
ASTM E1530
Processing Properties Metric English Comments
Cure Time 120 min
2.00 hour
Work Time
240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
Descriptive Properties Value Comments
Color White
Mix Ratio 20:1