Material Notes:
General Purpose: Two Part Adhesive and SealantComments: Low Viscosity Cure system: PlatinumInformation provided by NuSil
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
Viscosity 130000 cP
130000 cP
A
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength at Break 1.40 MPa
203 psi
Elongation at Break 110 %
110 %
Shear Strength 1.40 MPa
203 psi
Lap, Primed with CF1-135
Tear Strength 7.89 kN/m
45.0 pli
Thermal Properties Metric English Comments
CTE, linear 275 µm/m-°C
153 µin/in-°F
Thermal Conductivity 0.828 W/m-K
5.75 BTU-in/hr-ft²-°F
ASTM E1530
Processing Properties Metric English Comments
Cure Time 90.0 min
1.50 hour
Work Time
180 min
3.00 hour
Tack Free Time
10100 min

@Temperature 25.0 °C
168 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color White
Mix Ratio 10:1