NuSil CV-2510 Silicone, Two Part Adhesive and Sealant

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer NuSil
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NuSil CV-2510 Silicone, Two Part Adhesive and Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Purpose: Two Part Adhesive and SealantComments: Low/High Temperature, FlowableCure system: AlkoxyInformation provided by NuSil
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
Viscosity 45000 cP
45000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Tensile Strength at Break 4.10 MPa
595 psi
Elongation at Break 200 %
200 %
Processing Properties Metric English Comments
Cure Time 240 min
4.00 hour
Work Time
10100 min

@Temperature 25.0 °C
168 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color White
Mix Ratio 100:0.5