NuSil CF2-135 Silicone Primer

Category Fluid , Polymer , Thermoset , Silicone
Manufacturer NuSil
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NuSil CF2-135 Silicone Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Purpose: PrimersComments: Addition Cure SystemsCure system: HydrolysisInformation provided by NuSil
Physical Properties Metric English Comments
Specific Gravity 0.770 g/cc
0.770 g/cc
Solids Content 4.7 %
4.7 %
Viscosity 1.0 cP
1.0 cP
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 25.0 °C
1.00 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Clear