Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Northstar Polymers PAA-109 Curing Agent

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid
Manufacturer Northstar Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Northstar Polymers PAA-109 Curing Agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Northstar Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.024 g/cc
1.024 g/cc
Viscosity 600 - 1200 cP

@Temperature 71.1 °C
600 - 1200 cP

@Temperature 160 °F
Descriptive Properties Value Comments
Appearance at 25°C Clear Liquid with Slight Yellow Tint
Equivalent Weight 1094