Nitriflex Nitrilatex LVP-106 Vinyl Pyridine Styrene Butadiene Latex

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Nitriflex
Trade Name Nitrilatex
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nitriflex Nitrilatex LVP-106 Vinyl Pyridine Styrene Butadiene Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid. Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesives manufacture, fibers agglomeration, supported gloves manufacture, impregnation of non-woven, etc. Information provided by Dax Resinas
Physical Properties Metric English Comments
Solids Content 40 - 42 %
40 - 42 %
Method L-001/P-065; ASTM D1417
pH 10 - 11
10 - 11
25°C, Method L-003; ASTM D1417
Brookfield Viscosity 45 - 54 cP
45 - 54 cP
(spindle=1, 20 rpm); ASTM D1417
Mooney Viscosity 30 - 45
30 - 45
Method L-015; ASTM D1417, ASTM D1646
Surface Tension 46 - 55 dynes/cm
46 - 55 dynes/cm
Method L-005/L-040; ASTM D1417
Descriptive Properties Value Comments
Appearance Purple Liquid
Coagulum Content % 0-0.05
ASTM D1417; Method L-004
Cream Content g/150ml 0-0.03
Method L-013
Vinyl Pyridine Content g/150ml 13-15
ASTM D3533; Method B-016/B-028