Material Notes:
NITRIFLOW™ P-120 AD3 is a processing aid resin for PVC based on methyl methacrylate (MMA) and ethyl acrylate copolymer.Applications: Blow moulding process: packaging in general (bottles). Extrusion, calandering and thermoforming process: profiles, laminates in general, tubes, blister packs. Injection Process: technical goods. Foamed in general. Information provided by Dax Resinas
Physical Properties Metric English Comments
Volatiles 0.00 - 1.0 %
0.00 - 1.0 %
Method P-020
Descriptive Properties Value Comments
Retained in 60 mesh (aperture = 0.25) 0
Users viewing this material also viewed the following: