Nitriflex NitriClean N-685 NBR - Nitrile Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Nitriflex
Trade Name NitriClean
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nitriflex NitriClean N-685 NBR - Nitrile Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General use for technical artifacts that require resistance to oils and greases with good processability and low mold fouling. Applications: Rings, gaskets, joints. Information provided by Dax Resinas
Physical Properties Metric English Comments
Volatiles 0.00 - 0.70 %
0.00 - 0.70 %
Method B-003; ASTM D5668
Mooney Viscosity 45 - 55

@Temperature 100 °C
45 - 55

@Temperature 212 °F
ML1+4, Method B-002; ASTM D1646
Ash 0.00 - 0.50 %
0.00 - 0.50 %
ASTM D5667
Descriptive Properties Value Comments
Appearance Light to medium brown
Bound Acrylonitrile Content (%) 31 - 34
ASTM D3533
Mh (lbf.in) 28.0-48.0
ASTM D2084
ML (lbf.in) 5.0-12.0
ASTM D2084
Polymerization Cold
Tsl (min) 2.0-5.0
ASTM D2084