Nitriflex NP-2121 Powdered Nitrile

Category Polymer , Thermoset
Manufacturer Nitriflex
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nitriflex NP-2121 Powdered Nitrile.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General use for technical artifacts that require good resistance to oil and grease with good processability and transparence. Plastic modifier and impact modifier. Applications: flexible containers, sheets, sponge sports goods, shoes soles.Information provided by Dax Resinas
Physical Properties Metric English Comments
Volatiles 0.00 - 0.70 %
0.00 - 0.70 %
Method B-003; ASTM D5668
Particle Size <= 1000 µm
<= 1000 µm
99-100%; ASTM D1921
Mooney Viscosity 40 - 54

@Temperature 100 °C
40 - 54

@Temperature 212 °F
ML1+4, Method B-002; ASTM D1646
Descriptive Properties Value Comments
Bound Acrylonitrile Content (%) 31 - 34
ASTM D3533
CaCO3 Partitioning Agent Content % 10 to 14
Method B-035