Nitriflex NP-2007 Powdered Nitrile

Category Polymer , Thermoset
Manufacturer Nitriflex
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nitriflex NP-2007 Powdered Nitrile.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent performance at dynamic applications. Applications: hose tube, covers, belts, friction materials, rice dehusking roller, friction materials.Information provided by Dax Resinas
Physical Properties Metric English Comments
Volatiles 0.00 - 0.70 %
0.00 - 0.70 %
Method B-003; ASTM D5668