Material Notes:
Description: Polynil P240 HSLV was developed for injection molding applications, where a combination of heat aging resistance, abrasion resistance and impact strength is needed, such as chain tensioner guides.Key characteristics: High abrasion resistanceHigh heat aging resistanceAbility to absorb shock loads, also at low temperaturesInformation provided by NILIT.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Viscosity Measurement 240
240
relative viscosity (formic acid); ASTM D789
Mechanical Properties Metric English Comments
Tensile Strength, Yield 84.1 MPa
12200 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Tensile Modulus 2.70 GPa
392 ksi
ASTM D638
Flexural Strength 118 MPa
17100 psi
ASTM D790
Flexural Modulus 2.70 GPa
392 ksi
ASTM D790
Izod Impact, Notched (ISO) 6.93 kJ/m²
3.30 ft-lb/in²
ASTM D256
Charpy Impact Unnotched NB
NB
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 233 °C
451 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved