Material Notes:
Description: Polynil P100 is a grade has a viscosity that has been optimized for monofilament extrusion for high strength monofilaments.Key characteristics: Viscosity number 200 gr/cm3Excellent melt stabilityHigh elongation Information provided by NILIT.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Viscosity Measurement 100
100
relative viscosity (formic acid); ASTM D789
Mechanical Properties Metric English Comments
Tensile Strength, Yield 82.0 MPa
11900 psi
ASTM D638
Elongation at Break 72 %
72 %
ASTM D638
Tensile Modulus 2.80 GPa
406 ksi
ASTM D638
Flexural Strength 113 MPa
16400 psi
ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched (ISO) 6.09 kJ/m²
2.90 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 226 °C
439 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C
165 °F
ASTM D648