Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nilit FRIANYL B63 H-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Nilit (formerly Frisetta Polymer)
Trade Name FRIANYL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit FRIANYL B63 H-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Water Absorption 1.3 - 2.3 %
1.3 - 2.3 %
ISO 62
Water Absorption at Saturation 6.0 - 8.0 %
6.0 - 8.0 %
ISO 62
Viscosity Measurement 145
145
Viscosity index; ISO 307
Linear Mold Shrinkage 0.0060 - 0.013 cm/cm
0.0060 - 0.013 in/in
FRISETTA Test Method
Mechanical Properties Metric English Comments
Ball Indentation Hardness 160 MPa
23200 psi
ISO 2039-1
Tensile Strength at Break 160 MPa
23200 psi
ISO 527
Elongation at Break 4.0 %
4.0 %
ISO 527
Tensile Modulus 8.00 GPa
1160 ksi
ISO 527
Flexural Strength 200 MPa
29000 psi
ISO 178
Flexural Modulus 7.30 GPa
1060 ksi
ISO 178
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
DIN 53453
4.50 J/cm²

@Temperature -40.0 °C
21.4 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ISO 3146 DSC
Maximum Service Temperature, Air 115 °C
239 °F
Continuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 575 V
575 V
CTI 100; IEC 112
Users viewing this material also viewed the following: