Nilit FRIANYL B63 GV35 Nylon 6 for injection molding, 35% glass fiber reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer Nilit (formerly Frisetta Polymer)
Trade Name FRIANYL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit FRIANYL B63 GV35 Nylon 6 for injection molding, 35% glass fiber reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Water Absorption 1.5 - 2.4 %
1.5 - 2.4 %
ISO 62
Water Absorption at Saturation 6.0 - 7.0 %
6.0 - 7.0 %
ISO 62
Viscosity Measurement 145
145
Viscosity index; ISO 307
Linear Mold Shrinkage 0.0040 - 0.012 cm/cm
0.0040 - 0.012 in/in
FRISETTA Test Method
Mechanical Properties Metric English Comments
Ball Indentation Hardness 178 MPa
25800 psi
ISO 2039-1
Tensile Strength at Break 180 MPa
26100 psi
ISO 527
Elongation at Break 4.0 %
4.0 %
ISO 527
Tensile Modulus 10.0 GPa
1450 ksi
ISO 527
Flexural Strength 250 MPa
36300 psi
ISO 178
Flexural Modulus 8.10 GPa
1170 ksi
ISO 178
Charpy Impact Unnotched 5.50 J/cm²
26.2 ft-lb/in²
DIN 53453
NB
NB
ISO 179/1eU
5.00 J/cm²

@Temperature -40.0 °C
23.8 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eA
1.50 J/cm²
7.14 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ISO 3146 DSC
Maximum Service Temperature, Air 115 °C
239 °F
Continuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ISO 75
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 575 V
575 V
CTI 100; IEC 112