Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nilit FRIANYL A63 RV0 9005 Nylon 6.6 for injection molding

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant
Manufacturer Nilit (formerly Frisetta Polymer)
Trade Name FRIANYL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit FRIANYL A63 RV0 9005 Nylon 6.6 for injection molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6.6 for injection molding, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 2.2 - 3.0 %
2.2 - 3.0 %
ISO 62
Water Absorption at Saturation 8.0 - 9.0 %
8.0 - 9.0 %
ISO 62
Viscosity Measurement 145
145
Viscosity index; ISO 307
Linear Mold Shrinkage 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
FRISETTA Test Method
Mechanical Properties Metric English Comments
Ball Indentation Hardness 120 MPa
17400 psi
ISO 2039-1
Tensile Strength at Break 85.0 MPa
12300 psi
ISO 527
Elongation at Break 10 %
10 %
ISO 527
Tensile Modulus 3.60 GPa
522 ksi
ISO 527
Charpy Impact Unnotched NB
NB
ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179/1eA
0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
ISO 3146 DSC
Maximum Service Temperature, Air 130 °C
266 °F
Continuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 185 °C
365 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ISO 75
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 600 V
600 V
CTI 100; IEC 112
600 V
600 V
CTI-M 100; IEC 112