Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Niche Polymer PCABSN8BK PC/ABS

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced
Manufacturer Niche Polymer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niche Polymer PCABSN8BK PC/ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00600 cm/cm
0.00600 in/in
ASTM D955
Melt Flow 10.0 g/10 min

@Load 4.50 kg,
Temperature 260 °C
10.0 g/10 min

@Load 9.92 lb,
Temperature 500 °F
ASTM D123
Mechanical Properties Metric English Comments
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Elongation at Break 5.00 %
5.00 %
ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Unnotched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 112 °C
234 °F
ASTM D648
Vicat Softening Point 130 °C
266 °F
ASTM D789
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved