Niche Polymer PA66GF50BK Nylon 66, 50% Glass Fiber Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Niche Polymer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niche Polymer PA66GF50BK Nylon 66, 50% Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.000700 cm/cm
0.000700 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 235 MPa
34100 psi
ASTM D638
Elongation at Break 2.50 %
2.50 %
ASTM D638
Flexural Strength 390 MPa
56600 psi
ASTM D790
Flexural Modulus 14.5 GPa
2100 ksi
ASTM D790
Izod Impact, Unnotched 1.28 J/cm

@Thickness 3.17 mm
2.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 254 - 266 °C
489 - 511 °F
ASTM D789
Descriptive Properties Value Comments
Color Black