Niagara LaSalle 8620 Cold Finished Steel Bar

Category Metal , Ferrous Metal , Alloy Steel , AISI 8000 Series Steel
Manufacturer Niagara LaSalle
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niagara LaSalle 8620 Cold Finished Steel Bar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The most widely used carburizing alloy. Its nickel content imparts good toughness and ductility. The chromium and molybdenum increases hardness penetration and wearability. This steel's well balanced alloy content permits hardening to produce a strong, tough core and high case hardness. It machines at 110 sfm and has good welding qualities.Information provided by Niagra LaSalle Corporation
Component Elements Properties Metric English Comments
Carbon, C 0.18 - 0.23 %
0.18 - 0.23 %
Chromium, Cr 0.40 - 0.60 %
0.40 - 0.60 %
Iron, Fe 96.895 - 98.02 %
96.895 - 98.02 %
as balance
Manganese, Mn 0.70 - 0.90 %
0.70 - 0.90 %
Molybdenum, Mo 0.15 - 0.25 %
0.15 - 0.25 %
Nickel, Ni 0.40 - 0.70 %
0.40 - 0.70 %
Phosphorous, P <= 0.035 %
<= 0.035 %
Silicon, Si 0.15 - 0.35 %
0.15 - 0.35 %
Sulfur, S <= 0.040 %
<= 0.040 %