NextGen Adhesives G907-28 Potting Adhesive

Category Polymer , Adhesive
Manufacturer NextGen Adhesives
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NextGen Adhesives G907-28 Potting Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: NGAC G907-28 is a medium viscosity adhesive system formulated with a spherical glass filler to provide light weight and low shrinkage performance.Advantages and Applications: The NGAC G907-28 provides strong, light weight and durable bonds with minimal shrinkage upon cure. The NGAC G907-28 is easily mixed and cured at room temperature and provides excellent adhesion to glass, ceramic, metal and plastic.Information Provided by Nextgen Adhesives
Physical Properties Metric English Comments
Specific Gravity 0.800 g/cc
0.800 g/cc
Viscosity 33000 cP
33000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 45 min
45 min
Descriptive Properties Value Comments
Color Grey
Mix Ratio by Weight (R/H) 100/9