NextGen Adhesives EC907-34 Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer NextGen Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NextGen Adhesives EC907-34 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: NGAC EC907-34 is a two part, electrically conductive silver filled epoxy adhesive which can be cured at room temperature. It was designed for applications requiring excellent mechanical and electrical properties.Advantages and Applications: NGAC EC907-34 provides strong and high impact bonds which are electrically and thermally conductive. It bonds to a wide range of substrates including metals, glass and plastics. Additionally, the NGAC EC907-34 is highly resistant to chemicals.Information Provided by Nextgen Adhesives
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.0020 ohm-cm

@Temperature 65.0 °C
0.0020 ohm-cm

@Temperature 149 °F
0.20 ohm-cm

@Temperature 25.0 °C
0.20 ohm-cm

@Temperature 77.0 °F
Processing Properties Metric English Comments
Cure Time 120 - 240 min

@Temperature 65.0 °C
2.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 180 min
180 min
Descriptive Properties Value Comments
Color Silver
Mix Ratio by Weight (R/H) 100/6