Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Network Polymers
Trade Name Softflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers Softflex® UB 30 Black OEX.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 30
30
Instantaneous; ASTM D2240
Tensile Strength, Yield 26.2 MPa
3800 psi
Type 1 bar; ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
Izod Impact, Notched NB
NB
0.125 inch bar; ASTM D256
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
0.125 inch bar; ASTM D256