Material Notes:
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Melt Flow 8.1 g/10 min

@Load 1.00 kg,
Temperature 235 °C
8.1 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 65
55 - 65
Instantaneous; ASTM D2240
Gardner Impact >= 36.2 J

@Temperature -30.0 °C
>= 26.7 ft-lb

@Temperature -22.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Brittleness Temperature -50.0 °C
-58.0 °F
ASTM D746