Network Polymers Softflex® 4500

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Network Polymers
Trade Name Softflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers Softflex® 4500.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Melt Flow 1.5 g/10 min

@Load 1.00 kg,
Temperature 235 °C
1.5 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
11.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
11.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 40 - 45
40 - 45
ASTM D792
Tensile Strength, Yield 4.14 MPa
600 psi
chs 20 in/min; ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
Tear Strength 19.3 kN/m
110 pli
ASTM D624