Description: Polycarbonate, 10% Glass Filled BlackInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.8 MPa
9400 psi
chs 2 in/min; ASTM D638
Flexural Modulus 3.31 GPa
480 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
Test Method A (0.125 in bar); ASTM D256