Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Network Polymers Nylon 6609

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers Nylon 6609.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Natural NylonInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Water Absorption 1.2 %
1.2 %
24 hours Immersion; ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
1/8 in bar; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Yield 82.7 MPa
12000 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Strength 103 MPa
15000 psi
ASTM D790
Flexural Modulus 2.83 GPa
410 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
1/8 in specimen; ASTM D256
Tensile Impact Strength 210 kJ/m²
100 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
0.125 in bar; ASTM D648
Copyright © lookpolymers.com All Rights Reserved