Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Network Polymers NPP 50-0863

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers NPP 50-0863.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.963 g/cc
0.0348 lb/in³
ASTM D1505
Melt Flow 8.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.89 MPa
4335 psi
ASTM D638
Elongation at Break 1000 %
1000 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Tensile Impact Strength 101 kJ/m²
48.0 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Vicat Softening Point 194 °C
381 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746