Material Notes:
Description: Black Polycarbonate Polyester AlloyInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
24 hours at 73°F; ASTM D570
Water Absorption at Saturation 0.35 %
0.35 %
73°F; ASTM D570
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.8 MPa
7800 psi
chs 2 in/min; ASTM D638
Elongation at Break 27 %
27 %
ASTM D638
Flexural Modulus 2.18 GPa
316 ksi
Tangent (chs speed 0.05 in/min); ASTM D790
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
0.125 in bar, Unannealed/Conditioned 48 hours; ASTM D648