Material Notes:
NatureWorks PLA polymer 6060D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6060D is designed for extrusion into mechanically drawn staple fibers using conventional fiber spinning and drawing equipment. NatureWorks PLA 6060D can be used as a low melt binder polymer in a sheath-core confiation.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Melt Density 1.08 g/cc

@Temperature 230 °C
0.0390 lb/in³

@Temperature 446 °F
ASTM D1238
Viscosity Measurement 3.3
3.3
Relative Viscosity; CD Internal Viscotek Method
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 210 °C
10 g/10 min

@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
Mechanical Properties Metric English Comments
Elongation at Break 50 %
50 %
Fiber; ASTM D2256/ASTM D3822
Tenacity 0.309 N/tex
3.50 g/denier
ASTM D2256/ASTM D3822
Thermal Properties Metric English Comments
Melting Point 125 - 135 °C
257 - 275 °F
ASTM D3418
Glass Transition Temp, Tg 55.0 - 60.0 °C
131 - 140 °F
ASTM D3417
Processing Properties Metric English Comments
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Dew Point -35.0 °C
-31.0 °F
Drying Air Flow Rate >= 14.2 l/min
>= 0.500 ft³/min (CFM)